In a message dated 10/9/99 10:51:17 AM Central Daylight Time,
[log in to unmask] writes:
> Any one out there using Kester peelable solder mask, you know the pink
> stuff? We have noticed that it attacks metal. Dulls HASL land patterns,
> SMT fillets, attacks LPI mask (sometimes). In one case, where we use it
> to keep solder off of screw heads, rust formed where the zinc plate was
> missing.
> Comments?
Hi-dee ho there!
Sounds like you're using an ammoniated mask...there's a lot of temporary
peelable masks that will contain ammonia...that's what causing your problem.
Don't know what Kester formula your using (they have a few) but get one that
doesn't contain ammonia, if they have one. I use a Chemtronics peelable
mask...no problems thus far.
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|