Richard,
I am investigating Omikron now. Getting ready to do a proto run this
coming week.
I have not found anything to worry about with Omikron other then possibly
shelf life, which
is not a problem for me. We don't have large runs and turn board inventory
in a matter of
weeks. I have industry cohorts with first hand knowledge that say
IWT-Omikron is better than
ENIG in their opinions, so I am giving it a try to see if it eliminates the
problems I have with
OSP. I'm sure there are others who will say differently, but that is why I
am running the
prototype. The proof is in the performance for me.
I have heard about some problems with Dexter-FST, but not with Omikron,
which is why I am
trying it. There are also a lot of pro's and con's with Au, so IWT seems
like a potentially good replacement for OSP/HASL/ENIG, if it performs.
If you have some specifics on your statement that "neither work very well",
I'd be interested
in hearing what those specifics are.
Thanks.....DT
At 09:50 PM 10/22/99 -0700, you wrote:
>I understand there are (2) suppliers of the white tin
>process, but neither work very well. Does anybody
>think this technology is something my company should
>pursue, or just stay with Ni-Au?
>
>
>=====
>
>__________________________________________________
>Do You Yahoo!?
>Bid and sell for free at http://auctions.yahoo.com
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|