Scott,
There are many factors that will affect the distribution of solder on
your board from your pre-clean process all the way through hot air level.
Air knife angles and temperatures, normal dwell for an .062 panel is about 3
seconds. Depending on where your located, I can have someone come out and
help you get it running right, it won't cost you anything.
Just send me a direct e-mail and maybe I can even help you over the
phone.
Kind Regards,
Steve
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|