Hi TechNetters --
Anyone got any ideas/experience with cleaning (nondestructively!!) assembled
PWBs that were exposed to an electrical fire? The boards are covered with
soot and associated black gunk. They are conformal coated (urethane). TIA.
Sheila Smith, Marconi AES
##############################################################