Hollis Future ! ; what a blast from the past ; talking serious rural living
in Okla here;
Whoever wrote your procedure was a bit of .............
Our states 250'CENTIGRADE , +/- 5'C ; = FROM 240 TO 250 .
eASY FIX sTEVE = REWRITE THE PROCEDURE :
Validate window = say, 5x samples on low limit , 5y samples on high limit ;
random code :
x 1 4 5 7 9 y 2 10 3 6 8
1 2 3 4 5 6 7 8 9 10
mix ; sign off 610 or 001 visual inspection ; and ask your sharp QA to
distinguish x from y .
If they can not ; you're proven and can sail free again .
Nothing like fighting bull with logic mate ; don't give up , get even !
PK
PS
Sinking deeoooop hey ? , you better get back to civilization again .
Rat race it is ; beats slippery cowpastures (by a whisker)
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Thursday, 7 October 1999 4:05
To: [log in to unmask]
Subject: [TN] Wave solder pot temperatures...
Hi all!
It's been a frustrating day...
I was at our old wave solder machine this morning (a Hollis SMT Future-1,
about 12-years old) and one of our QA inspectors came in to check the
calibration on it. The procedure here is to verify that the speed of the
belt
is what's indicated on the readout of the machine, and to check that the
solder temperature in the pot is within +/- 5 degrees F (which seems
unnecessarily tight to me). from what is indicated. I run my pots a
485-degrees F. We were in the middle of a run, so she said that she'll do
the
belt speed check after we were through, but would go ahead and check the
solder temperature. We had the laminar pump running and she put the
thermocouple in the wave. The readout on the machine was 484 F., and she
indicated 490 F. on the hand held unit she was measuring with. She said;
"The
machine is out of calibration, your temperature is 6-degrees too high, it
needs to be re-cal'ed.." I told her it wasn't, that she should wait until we
finish the boards we were waving so I could shut the pumps off, let the pot
stabilize, and then she could take a reading. Her reply was (which I'm
getting so sick of); "That's not the way we do it around here..." ARRRRG! No
matter how much I tried to explain about the solder being pumped up to the
top to the wave formers and cooling down flowing back into the pot, then the
thermocouple in the pot sensing this, turning the heaters on to maintain the
set temperature and that's why the reading was a little high, I couldn't get
through to her...so I gave up.
But what's a realistic slop factor as far as the indicated temperature and
actual temperature of the solder. I think +/- 5-degrees F is way to tight, I
was thinking more like +/- 15-degrees....any opinions?
Thanks!
-Steve Gregory-
P.S. anybody need a good engineer?
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|