We coat a coupon an then meausure the thickness using an Electronic Thickness Gauge, manufactured by ETG 813.726.9225.
Pat Lujan
BFGoodrich Aerospace
505.938.5373
>>> David Hipp <[log in to unmask]> 09/30/99 03:33PM >>>
Good day. How do you measure conformal coating thickness, without sectioning
a board or a coupon? Which method (brush, dip, spray) has the best
repeatability for thickness?
We build board assemblies to IPC Class 2 and 3 and have no idea if we meet
the requirements of paragraph 10.1.2.1.
Regards,
Dave Hipp
Woodward Aircraft Engine Systems
Electrical Production Engineering
(815) 639-6732
FAX (815) 636-6040
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|