Ken
I am not an expert but.....If your minimum requirement is .001 and thickness is between .0004 and .001 you should reject. If your requirements are .001 then you should expect the manufacturer to produce that. If .0008 is now considered an acceptable thickness for you and you are willing to accept that then you need to change your specifications. In the mean time you have specified to your PCB manufacturer a very reasonable thickness and it should be met.
Tom Burek
-----Original Message-----
From: [log in to unmask] [SMTP:MIME :[log in to unmask]]
Sent: Wednesday, September 29, 1999 2:05 PM
To: [log in to unmask]
Subject: [TN] Hot: Copper plating thickness
<< File: ENVELOPE.TXT >>
-------------------------------------------------------------------------- --
If my requirement for the copper plating is 0.001" minimum (as spelled out
on my fab drawing) and if I am reading it between .0004"-.001", is it
rejects or not?. I tried to look at IPC-6012 which is calling out avg
copper
thickness. I don't how easy to get ave #. This is clearly a reject to me.
But I am looking for an expert opinion on the subject. Via Hole in
question
is 16 mil +3 mil / -10 mils.
re,
ken patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|