Eric,
We saw this problem years ago with our prep of the surface prior to
soldermask. What is your pre-mask prep?
Anne Ledger
EMDS, Inc.
> -----Original Message-----
> From: Eric Masters [SMTP:[log in to unmask]]
> Sent: Friday, October 01, 1999 3:06 AM
> To: [log in to unmask]
> Subject: [TN] Internal shorts
>
> I'm having a rather perplexing problem with shorts on inner layers.
> The
> short is very small, and occurs mainly on fine line jobs (5/5 mils and
> less).
> It also occurs primarily on layers with one ounce copper, although
> I've seen
> it on half ounce.
>
> The short is very very small; in fact, it is rarely seen at AOI.
> Usually, it
> is discovered at final electrical test. Failure analysis exhibits a
> very
> fine sliver of copper that appears to have broken loose from a trace;
> it
> remains attached at one end and flips across the adjacent circuit.
>
> Cross sections and SEM's of both developed resist and etched layers
> show a
> near vertical sidewall. Has anyone seen this phenomenon? Any
> suggestions?
>
> Eric
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|