TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Tue, 5 Oct 1999 13:05:35 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, pod <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Parts/Attachments:
text/plain (79 lines)
I resemble that remark.

Earl Grey Great Tea
----- Original Message -----
From: Ingemar Hernefjord (EMW) <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, October 05, 1999 9:52 AM
Subject: Re: [TN] Cold solder


> Earl Grey is a good tea, I agree,
> Now, Joan, are you sure it's about cold soldering at all? As you describe
it could as well be dewetting. If it's dewetting, your trouble shooting can
leave the wavesolder for a while. Again, I wonder why you don't do a wetting
test on the terminals.
> Good Lunch
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
> ----------------------------------------------------------------------
> Earl and all,
>
> the soldering was a lot better before. We've always had the QA on our
back,
> checking the flux density and the settings for the problem assemblies.
> Myself, I don't recall having seen so much cold solder.
>
> The machine had been calibrated last saturday during the monthly
> maintenance, when the pot is thoroughly cleaned.
>
> It's possible that the solder mask changed, since it's darker now.
Together
> with the soldering problems we started experiencing discoloration of the
> solder mask on the solder side. But wouldn't this randomly affect any
place
> on the surface? I still get the connectors OK, with bad solder joints on
the
> caps and resistor networks.
>
> There has been no artwork change. However, could some changes in the
> materials or manufacturing of the board affect somehow the thermal mass
here
> and there? I mean, maybe the connectors drain somehow the heat from the
> adjoining components.
>
> And anyway, what on earth generates cold solder in the waving process?
>
> Ioan
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2