Neil

Both materials could be suitable it depends on the type of environment
the component is to operate in. The zinc plated nut is probably cheaper
but my preferance to avoid possible galvanic corrosion problems with the
zinc and for appearance would be to use the stainless steel nut.  

regards
Chris Evans