TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Derek Humble <[log in to unmask]>
Date:
Tue, 5 Oct 1999 07:48:26 -0500
MIME-Version:
1.0
X-To:
"Tempea, Ioan" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Derek Humble <[log in to unmask]>
Parts/Attachments:
text/plain (114 lines)
                Ioan,
                I've got a few suggestions for you to check with respect to
your process.  Cold solder joints can be caused by incorrect solder
temperature, solder contamination, low preheat temperature, incorrect
conveyor speed and/or vibration and removing the board too early from the
wave.  A couple of other items to check are board and component
contamination.
                Best of luck,
                Derek Humble
                S.C. Process Engineering
                Brock Telecom Ltd.
                Tel. :(613) 498-3856 ext. 2428
                Fax  :(613) 498-3645
                E-mail: [log in to unmask]


                                -----Original Message-----
                                From:   Tempea, Ioan
[SMTP:[log in to unmask]]
                                Sent:   October 4, 1999 4:46 PM
                                To:     [log in to unmask]
                                Subject:        [TN] Cold solder

                        Hi Technos,

                        I'm in big trouble with a backplane.

                        It's a 13.5"x19.5", 3.7mm thick. The connectors are
disposed in parallel
                        lines, forming two columns a the two extremities. In
the middle we have no
                        components. In between the connectors there are some
TH caps and resistors.

                        ______________________________
                        ______                                ______  I
                        ______                                ______  I
                        ______                                ______  I
                        ______                                ______  I
                        ..                                          ..
                        ..
                        ______                                ______  I
                        _______________________________ I

                        For a long time the soldering was OK, with small
problems in the four
                        corners ( a couple of holes not 100% full).

                        For about a week or so, the solder joints of many
caps or resistors present
                        cold solder. There are no significant cold solder
problems with the
                        connectors, which present though a little less
wetting (some of the fillets
                        are not what they used to be).

                        The question is: why do I get the cold solder and
how can I get read of it?

                        We use :
                        - no-clean technology
                        - Multicore Sn63 solder
                        - Multicore X33 flux
                        - strong radiation preheating ( two top preheaters
at 700F and two bottom at
                        750F); we spent a lot of time tweaking to avoid
damaging the board
                        - two passes, one for fluxing only, no wave, the
second one right after with
                        no fluxing, but with wave
                        - no chip wave (that's what I have, hehehe), just
omega on our Electrovert
                        Econopak II

                        Any help would be greatly appreciated.

                        Thanks,      Ioan


##############################################################
                        TechNet Mail List provided as a free service by IPC
using LISTSERV 1.8c

##############################################################
                        To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in
                        the body:
                        To subscribe:   SUBSCRIBE TECHNET <your full name>
                        To unsubscribe:   SIGNOFF TECHNET

##############################################################
                        Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for additional
                        information.
                        If you need assistance - contact Gayatri
Sardeshpande at [log in to unmask] or
                        847-509-9700 ext.5365

##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2