TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Wanner Bernhard <[log in to unmask]>
Date:
Wed, 20 Oct 1999 17:47:32 +0200
X-To:
Manon Dutil <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Wanner Bernhard <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
Manon,
At table 4-12 the header of four column (between "Materials" and
"Reference") says four time the same: "a0". I would expect four different
material properties (together with their metric).
Bernhard


        -----Ursprüngliche Nachricht-----
        Von:    Manon Dutil [SMTP:[log in to unmask]]
        Gesendet am:    Mittwoch, 20. Oktober 1999 17:26
        An:     TechNet E-Mail Forum.; Wanner Bernhard
        Betreff:        Re:      [TN] IPC-HDBK-001

        Bernhard,

        Table 4-12 header in the IPC-HDBK-001 is "Temperature constants ai
of
        coefficient of Thermal Expansion (ppm/3C) of some Electronic
Packaging
        materials"

        If that is what you are looking for...

        Manon


##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2