TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Jonathan Whitcomb <[log in to unmask]>
Date:
Tue, 19 Oct 1999 11:24:50 -0400
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (28 lines)
I'm don't think it makes sense to specify a class 3 annular ring requirement (1
mil annular ring) just because you have a high reliability application.  My
feeling is class 2 with some breakout allowed (provided minimum spacing to
adjacent line is OK and line entry to land is adequately flared) will last
forever for 99% of applications.  A class 3 annular ring only makes sense for
some kind of application (military?) which sees huge temperature swings.   By
blanket specifying class 3 for a commercial/ordinary application because you
want high reliability, you are getting overkill on the annular ring requirement
and unnecessarily impacting manufacturability.

Jonathan Whitcomb  IBM Endicott   607-757-1326   [log in to unmask]
Dept T49G bldg 257-2  1701 North St.  Endicott NY 13760   aisle H office X013
pager 2930  fax 607-757-1156

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2