TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Carey Pico <[log in to unmask]>
Date:
Tue, 19 Oct 1999 10:47:08 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bogdan Gabi <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-8"
From:
Bogdan Gabi <[log in to unmask]>
Parts/Attachments:
text/plain (143 lines)
thank you very much!
Gaby

> -----Original Message-----
> From: Carey Pico [SMTP:[log in to unmask]]
> Sent: ג אוקטובר 19 1999 0:56
> To:   [log in to unmask]
> Subject:      Re: [TN] TIN/GOLD alloy
> 
> There are many practical problems in discussing solder compounds: 1) when
> does one talk about "equilibrium" compositions/phases when one has
> nonuniform thermal processing (heat/cool), 2) interface metals not fully
> dissolved, 3) gaseous and liquid (flux) impurities, and 4) reliable aging
> tests.
> 
> That said, here is my comments on tin-gold:
> The issue with using gold is the occurance of the crystal structure of the
> AuSn4 phase depending on the solder mix, about 220C melting/liquidus/phase
> change point. Above a critial value (approximately 5% Au for Pb37-Sn63 wt%
> or ~10% Au for pure Sn), the crystal structure becomes large grained.  The
> the poor interfacial properties between AuSn4 crystals tend to dominate
> the
> mechanical strength, leading to embrittlement.  (For the record, at lower
> percentages of Au, you still have AuSn4 crystals, only that they are
> fine-grained and are dispersed in the Pb-Sn mix.  In fact, they can
> increase
> the quality of the joint by "pinning" the Pb-Sn grains from moving without
> much plastic flow).  So soldering to pure Au with Pb-Sn (or pure Sn) is
> going to get you into trouble.  Track down some of the past work on TAB
> bonding to Au-bumped Si substrates (sorry, I don't have any references to
> start you on).
> 
> Still I'm confused about the original memo (below in a mail response).  If
> you are soldering to gold, you are starting from the worst alloy in using
> AuSn4, the most brittle form of Au-Sn.  If you want to solder to gold, use
> a
> gold-dominated solder (e.g. Au5Sn).  But these are in the 400C+ melt
> region.
> These are typically used as initial/tack-down solder step or in packaging?
> If so, then they can go through a secondary soldering (Pd-Sn) step at 200C
> without
> noticeable damage (assuming the Pd-Sn is not applied to the Au area).
> 
> Any comments from the peanut gallery?
> Carey
> -----Original Message-----
> From: Jack Crawford <[log in to unmask]>
> To: [log in to unmask] <[log in to unmask]>
> Date: Sunday, October 17, 1999 3:06 PM
> Subject: Re: [TN] TIN/GOLD alloy
> 
> 
> >Gaby, et al
> >
> >Don't forget that IPC also has a leadfree website http://www.leadfree.org
> and we are
> >hosting a leadfree e-mail forum (like technet) also.  More info on that
> website.
> >jack
> >
> >>>> Gabriela Bogdan <[log in to unmask]> 10/17/99 03:00PM >>>
> >Dear TechNetters!
> >Please could you comment on the use of Tin/Gold 90/10 solder ?
> >The application is for microwave applications when soldering to gold.
> >Its melting temp. is 217C .
> >I have the following questions:
> >How does this composition correlate with the maximum gold content in a
> >solder joint?
> >Would it be possible to pass such a subassembly through a secondary
> >reflow with 63/37 Tin/Lead?
> >Is it recommended ONLY for soldering to gold?
> >It must be very expensive too??!!
> >Paul, Werner, my apologies.
> >Thank you
> >Gaby
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> >the body:
> >To subscribe:   SUBSCRIBE TECHNET <your full name>
> >To unsubscribe:   SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >information.
> >If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> >847-509-9700 ext.5365
> >##############################################################
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> >the body:
> >To subscribe:   SUBSCRIBE TECHNET <your full name>
> >To unsubscribe:   SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >information.
> >If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> >847-509-9700 ext.5365
> >##############################################################
> >
> 
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2