TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Date:
Fri, 15 Oct 1999 21:09:22 EDT
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (31 lines)
In a message dated 10/15/99 7:43:40 PM Central Daylight Time,
[log in to unmask] writes:

> Also, the liquidus for Sn70 is only 378 deg C (vs. 361 deg C for Sn63)
>
>  Timothy,
>
>  Don't ya' mean fahrenheit?
>
>  -Steve Gregory-

Also, ya'll can go to: http://www.indium.com and then click on: "Specialty
Solders & Alloys, Technical Chart and information" for a few charts of the
characteristics about a whole mess of different alloys...

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2