I have in the past placed on the TECH NET, addressing a manufacturer of a No
Clean Solder Paste. The problem that was being addressed was Lot to Lot
inconsistency. The manufacturer of this no clean paste has been very
supportive to help us to get to the root cause of our problem. They have
given us very good technical support. We are focusing in on our problems
with the help of Alpha Metals. I am publicly apologizing for the way that I
have handled this anomaly.
Donn E Steffen
Senior Quality Engineer
VDO Control Systems
Auburn, IN 46706
Phone (219)925-8887
Fax (219)925-8710
Email: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|