Steve & Kelly,
Check out the work being done by the CCAMTF (Circuit Card Assembly and
Materials Task Force) They evaluated a number of combinations of surface
finishes conformal coatings and other factors (not sure about laminate) in
various environments including diesel fuel and hydraulic fluid.
Contact Ronald L. Iman w/ Southwest Technology Consultants.
[log in to unmask]
http://ourworld.compuserve.com/homepages/ron_iman
or Jeffery F. Koon w/ Raytheon
[log in to unmask]
CCAMTF is a joint industry task force and they presented at the last IPC
conference on surface finishes.
Scott
-----Original Message-----
From: Kelly M. Schriver [mailto:[log in to unmask]]
Sent: Monday, October 11, 1999 3:50 PM
To: [log in to unmask]
Subject: Re: [TN] Fuel resistant laminate...
Yo Steve -
I hit the books this weekend on your fuel resistance question, and pretty
much drew a blank. I'm not certain that anyone is trying to directly
immerse a PC Assembly into a fuel tank without either protecting it with a
metal enclosure or a fuel resistant dip coat.
I have used several fuel resistant coatings and sealants over the years -
Goodyear Aerospace comes to mind -- you might take a look on the web in
their area.
I'll keep diggin and pass on anything I turn up.
Regards - Kelly
-----Original Message-----
From: Stephen R. Gregory <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Monday, October 11, 1999 7:53 AM
Subject: [TN] Fuel resistant laminate...
>Mornin' everybody!
>
>Well, here I am at the ol' salt mine. Thanks to everybody who replied to my
>"blowin' off some steam" email. There was a lot of good advice. I would
like
>to be able to sit down make some "whiz-bang" presentations to convince
>certain people about changing things, but the fact of the matter is, I flat
>don't have the time. Too busy fighting fires...but I really don't want to
get
>into all that again.
>
>Anyway, I was asking again if there's any recommendations for a good
laminate
>material to use that will withstand fuels, and a coating to use to cover
the
>electronics on it. I've got my Clyde F. Coombs Jr. book and will be pouring
>through the pages.
>
>This is supposed to be used for a fuel quantity indicating system...
>
>Thanks! Try and have a great Monday guys, I'm gonna...
>
>-Steve Gregory-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|