Nancy, also some reference like:
a) ASTM G 1-81. Standard practice for preparing, cleaning and evaluating corrosion test specimens.
b)ASTM G 16-71. Recommended practice for analysis of corrosion data.
c)ASTM G 50-76. Recommended practic for conducting atmospheric corrosion tests.
d)IEC 68-2-42 and -43 SO2 and H2S tests.
e)IEC 68-2-60. Environmental testing procedures for very low concentration of polluting gases.
f)as a whole, IEC has a lot of documents about migration, corrosion and environment. Not much used by americans.
g)ASM Handbook n:o 13 "Corrosion" is my own bible. 100 years experience in one book! Cheep. Can also be used as pillow when your concentration
migrates.
Good Luck /Ingemar
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|