Hi All
Does the "cured" adhesive used to secure surface mount components
to the bottom - wave solder - side of a board flow during wave solder
operations?
I am trying to find out how/when the adhesive got inside the crack on a
cracked
resistor. My impression was that the cured adhesive would not move????
Susan Mansilla
Robisan Lab
##############################################################