Sorry Julie I didn't realise you were refering to a HASL pot.
Ken
(Embedded
image moved Julie Dixon <[log in to unmask]>
to file: 10/07/99 01:59 PM
pic18326.pcx)
To: [log in to unmask]
cc: (bcc: Kenneth Kirby/ElectrovertUS/Cookson)
Subject: [TN] HASL-contaminated solder pot
TechNet,
We have sporadic problems with the copper level rising in our solder pot.
We
reduce the temp and dross each morning. Could you recommend a specific PM
program to keep our SnPb clean? We believe per the certicates of analyses
that
our supplier gives us good product. Any other reasons it might rise?
Thanks,
Green
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################