TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Thu, 7 Oct 1999 13:24:55 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bogdan Gabi <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-8"
From:
Bogdan Gabi <[log in to unmask]>
Parts/Attachments:
text/plain (98 lines)
Dear Ingemar,
sorry to add some "garbage" mail to the many replies, but you are wrong
about the green Chartreuse!
Ioan is dreaming about a nice glass of PALINCA right now, or am I wrong?
Gaby

> ----------
> From:         Ingemar Hernefjord
> (EMW)[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Ingemar Hernefjord (EMW)
> Sent:         ?יום רביעי 06 אוקטובר 1999? 14:48
> To:   [log in to unmask]
> Subject:      Re: [TN] Cold solder epilogue... maybe
> 
> Interesting, Juan...
> 
> by the way, did you make the wetting test? I'm curious.
> And what's wrong with tea, you need sip something besides the green
> Chartreuse.
> See you Huan..
> 
> Ingemar
> 
> 
> -----------------------------------separator------------------------------
> --
> 
> Thanks for the interest and thoughtfulness.
> 
> There are three things I would like to clarify:
> 
> - first, my identity, the name is IOAN, starts with an I, the letter after
> H. Some of you passed this test;
> 
> - second: tea, grog, etc is not exactly my kind of stuff; where I come
> from
> we go for strong licors;
> 
> - third: looks like the hours I spend reading through e-mails are very
> precious. Being in contact with people of your expertise is a big chance
> for
> me.
> 
> So, after getting some of the hints on the Technet, I realized that,
> indeed,
> it's not cold solder, but the dull, grainy joints that IPC-610 accepts for
> this kind of boards.
> 
> Did this solve my problem? Maybe. Now I have this phenomenon labeled as
> process indicator by the QA. This adds to the other process indicator, the
> solder joints that don't have 100% filling. The same IPC-610 accepts 50%,
> so
> we are going to make some cross sectioning.
> 
> The thing is I have two process indicators that are getting worse. More
> grainy joints, more not-so full joints. I wonder where will this lead.
> 
> Why do we do two passes? We couldn't avoid damaging the board with only
> one
> pass, simply, the board wouldn't preheat enough to avoid the thermal shock
> when hitting the wave. If we set the preheaters higher, the passive
> components will go out of spec.
> 
> Thanks again,
> 
> Ioan
> 
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
> 

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2