Miguel
Solder balls/splashes??!!! We're using a VOC free water
based flux for wavesoldering and Kester 951 for hand soldering. We've had
instances where repair operators use the water based flux for repair, I
know, I know, molten solder and water don't mix well. To continue, you may
want to try baking the boards to remove moisture trapped inside and/or limit
the amount of flux being used by repair people, flux pens work well.
Derek Humble
S.C. Process Engineering
Brock Telecom Ltd.
Tel. :(613) 498-3856 ext. 2428
Fax :(613) 498-3645
E-mail: [log in to unmask]
-----Original Message-----
From: Miguel Vallejo
[SMTP:[log in to unmask]]
Sent: October 6, 1999 10:46 PM
To: [log in to unmask]
Subject: [TN] FW: solder
balls/splashes
Are there any assembly audience out there besides
me?
> ----------
> From: Miguel Vallejo
> Sent: Monday, October 04, 1999 6:13 PM
> To: [log in to unmask]
> Subject: solder balls/splashes
>
> Hi,
> Is anyone out there having problems with solder
balls and splashes in
> your hand soldering process using no clean
solder/flux?
> We've been using Kester SN63PB37 alloy solder,
QQ-S-571-F-WLRP-1, and
> 961 flux, in our application and found that it
produces solder
> splashes and solder balls.
> Is there a way of preventing this condition?
>
>
##############################################################
TechNet Mail List provided as a free service by IPC
using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri
Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|