Tom,
One thing you need to add to your call-out is whether thickness is base or
finished.
MIL was a base material thickness wereas IPC can be either.
If you call out IPC finished remember to add plate up and mask thickness.
I would suggest using 0590 as the base thickness
Hope it helps
FNK
Frank N Kimmey, C.I.D.
EM Designer
Honeywell Security Products
916-353-5366
[log in to unmask]
> ----------
> From: Tom Reilly[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Tom Reilly
> Sent: Wednesday, October 06, 1999 9:21 AM
> To: [log in to unmask]
> Subject: [TN] Plating Thickness
>
> We need some expert assistance using the IPC-4101 specification for
> fabricating bare boards. The group seems to have very knowledgeable
> fabricators
> and designers. Please take some time and help a new member to the group
> help us
> fabricate board more reliably.
> We recently had problems with bare boards coming in too thick (.070 -
> .072).
> I would like to know what the minimum and maximum thickness the card
> should be
> using the following specification. (Specification used "MATERIAL: GFN 0620
> C1/C1
> A2A per MIL - P - 13949F"). To ensure we receive boards that are .062 +/-
> .005
> how should the specification read and why. (Others have suggested GFN 0590
> C1/C1
> A2A).
>
> Current specification used:
> GFN 0620 C1/C1 A2A spec is as follows:
> 0.0000 GFN = FR4 material with no color added.
> 0.0620 0602 = .062 thick base material without copper
> 0.0030 C1/C1 = 1oz. copper each side
> 0.0000 A2A = Quality issues not effecting thickness
> 0.0030 60/40 Tin Lead
> 0.0020 Solder masking (LPI)
> ----------
> 0.0700 Total thickness Max.
>
>
> We would like to start using IPC-4101 specification in our fabrication
> control drawings. To accomplish the preferred result of .067 +/- .005 here
> are
> the specification we derived from the 4101. Please your recommendations on
> how
> we can get yields with our preferred PCB thickness (IPC-4101 K21 0620
> C1/C1 KA),
> (IPC-4101 L21 0590 C1/C1 AA) or other.
>
> Maximum dimension specified:
> IPC-4101 K21 0620 C1/C1 KA spec is as follows:
> 0.0000 K21 = FR4 material with no color added.
> 0.0620 0620 = .062 thick base material with copper
> 0.0000 C1/C1 = 1oz. copper each side
> 0.0000 A2A = Quality issues not effecting thickness
> 0.0030 60/40 Tin Lead
> 0.0020 Solder masking (LPI)
> ----------
> 0.0670 Total thickness Max.
>
> IPC-4101 L21 0590 C1/C1 AA spec is as follows:
> 0.0000 L21 = FR4 material with no color added.
> 0.0590 0590 = .059 thick base material without copper
> 0.0030 C1/C1 = 1oz. copper each side
> 0.0000 A2A = Quality issues not effecting thickness
> 0.0030 60/40 Tin Lead
> 0.0020 Solder masking (LPI)
> ----------
> 0.0670 Total thickness Max.
>
> How do you build multi-layer cards using IPC-4101 specification. Our
> intent
> is to build boards with the same thickness as the double sided by using
> the
> IPC-4101 specification with one ounce copper on external layers and one or
> half
> ounce internal layers. We have difficulty extracted this information from
> the
> IPC-4101 document. Please enlighten me with your expert knowledge by
> sending
> build-up of the specification similar to the specification s shown above.
> Thanks
> in advance for your much needed help.
>
>
> Thanks,
> Tom
> Document Services Manager / CAD Manager
> Inter-Tel Integrated Systems, Inc.
> 7300 W. Boston Street
> Chandler AZ. 85226
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|