Martin:
Beware!!!!! I used dummy BGA's to verify the reflow profiles and had INVALID results.
Using the dummy parts I saw shorts/opens/... (using x-ray's). After several months I
realized the dummy
components did not perform the same as REAL parts with die's. My advise is to ask your
supplier for BGA's
that failed functionally and run your test with these parts.
Chris
Martin Hart wrote:
> Dear Michael Jermias, the TopLine distributor in Germany will be very happy
> to assist you with dummy BGA and SBGA, and ESBGA and test boards. The
> TopLine distributor is TEKELEC in Munchen. Their telephone number is
> 089/5164-154. In the USA TopLine's telephone is (800) 776-9888. email is
> <[log in to unmask]> Website is http://www.toplinedummy.com
>
> At 01:59 PM 10/5/99 +0200, Jeremias, Michael wrote:
> >> Ladies and Gentlemen,
> >>
> >> we want to start another program for reliability tests with assembled
> >> PCBs with BGAs etc.
> >>
> >> Who can help us with :
> >>
> >> 1.
> >> dummy components for the following package types:
> >>
> >> ESBGA
> >> SBGA
> >> BGA
> >> CBGA
> >>
> >> approx. 750 joints resp. more than 45 mm square
> >>
> >> 2. appropriate test printed circuit board
> >>
> >> 3.appropiate underfiller for large BGAs suited also for noclean solder
> >> processes.
> >>
> >>
> >>
> >> Thank You very much
> >> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|