Enid,
Our drawings call out 30 microinches minimum thickness of gold and 150
microinches minimum thickness of nickel for gold edge contacts.
This was established in coordination with our PWB vendor (see, that does
happen sometimes!)
-Steve
Steven K. Lustig
Process Engineer
EMS Technologies, Inc.
Norcross, GA
(770) 263-9200 x4714
[log in to unmask]
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Thursday, September 30, 1999 4:58 PM
To: [log in to unmask]
Subject: [TN] PWB edge contact metallization
Importance: High
What is the recommended metallization for a gold edge contact in a pwb?
Regards,
Enid
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|