Francis,
What does your Hull cell panel look like?
Eric Yakobson
Alpha PC Fab
Francis Lai <[log in to unmask]> on 09/15/99 10:35:00 PM
To: [log in to unmask]
cc:
Subject: [TN] Dull finish around holes in Cu plating
We are using pattern plating. After carbon treatment of our acid plating
bath, we ran dummies for 2 hours then plate our panels. However the area
around the holes showed dull and slightly rough finishes. The areas
which have no holes showed shiny. We use the plating bar method. We
etched the pattern and then use platting bar for connections. We ran two
panels in a bath which was not carbon treated and they were fine. The
PTH walls looked dull and slightly rough too. Can anyone help?
My e-mail : [log in to unmask]
Thanks!!!!!
Francis
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################