<< We are currently having to mask off on a typical board, 4 x 4.5mm hole
with large lands, 1x3mm hole with large land, 3x1.5mm hole & 4 pads for
LED's.
All but the LED's are too big for screened on peelable resist (drips
through), and we cannot apply that to the SMT side. >>
Matthew,
In my previous experience this would not be a problem at all for a PVA
coating system to selectively coat, then cure. The main issue to consider is
the smallest spacing between things that must be coated and things that must
be left uncoated. I worked with spacings as small as .020 without much
problem.
Jon Moore
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|