Tom,
What is turpene?
Do you mean turpentine or terpenes?
Either of these does have its problems. Shoot, an MDS for water would
probably show it as an asphyxiant!
regards,
Bev Christian
Nortel Networks
> -----Original Message-----
> From: Tom Colton [SMTP:[log in to unmask]]
> Sent: Tuesday, September 07, 1999 9:33 AM
> To: [log in to unmask]
> Subject: Re: [TN] Flux Removal with MEK
>
> Turpene works reliably well, and the MSDS shows no known hazards.
>
> TC
>
> Kathie Lucas wrote:
>
> > David,
> >
> > At my company I have been asked to look into replacing MEK with
> something
> > less hazardous and just as effective. So far I haven't found anything.
> I
> > am not giving up on this. Justification on why not to use this is easy,
> > just read the MSDS.
> >
> > "Extremely flammable. Inhalation may cause irritability to the nose and
> > throat. Concentration above the TLV may cause headache, dizziness,
> nausea,
> > shortness of breath and vomiting. High concentration may cause central
> > nervous system depression and unconsciousness. Ingestion may cause
> > irritability to digestive tract with abdomen spasms, nausea and
> vomiting.
> > Large doses may cause narcosis. May cause irritation and discoloration
> to
> > skin. Vapors or irritation to eyes. Splashes may produce painful
> > irritation and eye damage. Prolonged skin contact may produce
> dermatitis."
> >
> > This product is not listed by IARC, NTP or OSHA as a carcinogen. Why I
> do
> > not know. Look at everything it does to the human body.
> >
> > Methyl-ethyl-ketone is not listed in Schedule 1 of the Ozone Protection
> Act
> > 1989 of the Commonwealth, and therefore this substance is not regulated
> in
> > the ACT under the Ozone Protection Regulations 1997.
> >
> > I have been talking with a company called Enviro Tech. Their number is
> > 1-708-343-6641 contact name--Dan Duerkop.
> >
> > Kathie Lucas
> > L-3 Communications
> > [log in to unmask]
> > 1-801-594-3394
> > > -----Original Message-----
> > > From: David Hipp [SMTP:[log in to unmask]]
> > > Sent: Thursday, September 02, 1999 9:25 AM
> > > To: [log in to unmask]
> > > Subject: [TN] Flux Removal with MEK
> > >
> > > TechNetters - some of our assembly techs use MEK to remove flux. I
> know
> > > MEK
> > > is potent and probably shouldn't be used for flux removal. What I need
> is
> > > some justification WHY we shouldn't use MEK.
> > >
> > > We are soldering 22 gauge stranded wire to connector lugs and
> microswitch
> > > turret terminals. This assembly is part of a fuel control for
> commercial
> > > fanjet engines. We use Sb5WS (Tin 94%, Lead 0.2%, Antimony 4-6%)
> solder
> > > and
> > > Kester 197 Flux, which is type RMA.
> > >
> > > Any help is appreciated.
> > >
> > > Regards,
> > > Dave Hipp
> > > Woodward Aircraft Engine Systems
> > > Electrical Production Engineering
> > > (815) 639-6732
> > > FAX (815) 636-6040
> > >
> > > ##############################################################
> > > TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> > > ##############################################################
> > > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > > following text in
> > > the body:
> > > To subscribe: SUBSCRIBE TECHNET <your full name>
> > > To unsubscribe: SIGNOFF TECHNET
> > > ##############################################################
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > > additional
> > > information.
> > > If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or
> > > 847-509-9700 ext.5365
> > > ##############################################################
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> > 847-509-9700 ext.5365
> > ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|