hi,
i assume you have a universal lead forming die of some sort. you surely
don't want to trim and form with hand tools. so, you'll need to trim and
form the parts before tinning for two reasons. first, the tinning can goof
up your lead forming and trimming die. second, the tie bar is going to give
you a lot of grief when you dip the leads into a solder pot, or wave, or
whatever.
our assembly operators are experts at hand tinning these parts (forget about
asking us to do them). it can be done, but it's tedious; and your operators
might not talk to you afterwards. i'd definitely lean towards getting them
done 'outside'.
phil
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, September 28, 1999 4:35 PM
To: [log in to unmask]
Subject: [TN] Pre-Tinning Fine Pitch...
Hi ya'll!
Boy, I may have quite a task ahead of me. There's this assembly that has hit
the floor that has just about every part (CQFP's and ceramic SOIC's) in the
un-formed state, and we've got to form and trim, then Pre-tin the gold
plated
stuff. I've already got a call into Six Sigma to get a quote on doing this
stuff for me, but it may turn-out that we won't have the time to deal with
this build and sub-contracting the forming and trimming, and pre-tinning out
(what's new?).
But in case I have to pre-tin the CQFP's myself, are there any tips that
anyone can share to help me get through this as painlessly as possible?
These
parts are 320-pin 25-mil pitch and still have the tie-bars attached. I've
got
a bottle of nitrogen and plan to "Rube-Goldberg" me an enclosure to blanket
the pot with nitrogen over the tinning pot that I'll be using...I think
that'll help to cut down on the bridging I'll see. I'm going to use an RMA
flux as well...any other suggestions? PLEASE?
Thanks!
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|