Allen,
Is this a component which was designed as a through hole and afterwards went through
lead forming for smt?
I ask you because you said that the leads are round.
If so, your main problem should be coplanarity of the leads and solderability, I think.
I would look only for solder height - reaching the 1/2 of the lead diameter on all
leads should be fine.
If there is no bending, the solder joint should have a nice meniscus and not touch the
component body.
I hope this helps.
Gaby
"Kluz, Allen E." wrote:
> This is on the top side of the pcb, using a surface mount part. I have the
> '94 IPC 610 book, looking on pg. 123, under SMT assy.
>
> Sorry, your drawing doesn't help for my application.
> > -----Original Message-----
> > From: Nancy Trumbull [SMTP:[log in to unmask]]
> > Sent: Friday, September 17, 1999 11:19 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] maximum solder joint thickness
> >
> > Hi Allen,
> > I would like to help you but I'm not sure about your question.
> > Please give a little more information.
> > 1. What side of the PCB
> > 2. Plated through or not
> > 3. Joint = Solder thickness yes
> > 4. What page are you looking on
> >
> > Your question is how thick can the solder be from the pad to
> > the lead.
> > Please open the attachment and let me know if this is what your
> > are asking.
> > Jack Crawford will know I'm sure
> > Or e-mail me
> > [log in to unmask]
> >
> > Nancy
> > >>> "Kluz, Allen E." <[log in to unmask]> 09/17/99 10:42AM >>>
> > Technetters,
> > I've been searching through the IPC-A-610: Acceptability of Electronic
> > Assemblies Guidelines, and can't find anything on guidelines for maximum
> > joint thickness (from the pad to the lead). The manual refers to as the
> > "G"
> > dimension, which clearly identifies the minimum thickness'. Does anyone
> > know of guideline for this and where it's stated? I'm looking for a round
> > lead in particular.
> >
> > Thanks in advance.
> >
> >
> > Allen Kluz
> > Supplier Quality Engineer
> > [log in to unmask]
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> > 847-509-9700 ext.5365
> > ##############################################################
> > << File: Joint.doc >>
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|