In my papers on double sided reflow and Intrusive Soldering, I use the
formula:
Weight of component in grams
total pad to lead mating surface area (in inches)
and if the result is < or equal to 30 grams, the component will not fall off.
Last week, at the SMTA Int'l conference in San Jose, Bob Willis and I
compared further notes and experience on this. We have both used components
that exceeded 30 grams/in sq but we are sticking with this number. This
incorporates a lot of components including most fine pitch QFPs, TSOPs, as
well as 68 pin PLCC. Trouble components are larger mass components and many
ceramics including some large tantalums. So experiment with any component
first.
It also assumes that you have a smooth running reflow oven conveyor - no
"shake and bake".
Regards,
Phil Zarrow
ITM, Inc.
Durham, NH USA
www.ITM-SMT.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|