TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Dave Hoover <[log in to unmask]>
Date:
Fri, 3 Sep 1999 14:09:44 -0700
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Hoover <[log in to unmask]>
Parts/Attachments:
text/plain (93 lines)
According to the IPC Expo Paper in '99,
"Meeting Fine Pitch Assembly Needs with a Solderable Tin 
Finish", by David Ormerod, The FST finish passed the
Siemens (Whisker Test) DIN41640 - 56 days @55'C/20%RH
(also long study tests of 35-45'C@85-93%RH). No Whiskers
were found.

Groovy
-----Original Message-----
From: Jerry Cupples [mailto:[log in to unmask]]
Sent: Friday, September 03, 1999 1:47 PM
To: [log in to unmask]
Subject: Re: [TN] Whiskers Problem on Leadframes


Stephané Menard asked:

>I have a question regarding the well known problem of whiskers generation
on
>leadframes.
>
>With the concept of lead free deposit and the investigation of several
>alternatives   (Sn-Bi, Sn-Ag, Pure Tin, etc..) to Tin-Lead, we need to
study
>the risk of generation of whiskers with those substitutes.
>It is generally agreed that Tin alloys (even at low percentage in the other
>metal) are not prone to this problem whereas pure Tin deposits are.
>
>However, does anybody have a recognized method (electrochemical, physical,
>etc...) which could help in predicting the apparition, or not, of this
>problem (besides the standard aging test which sometimes can be quite
>doubtful !) ?
>
>I am looking forward to your answers and comments.

Michael Carano offered an interesting reply which concurs with my
experience, and also:

There is a method in which the electroplated coating is applied to thin
coupons which may be measured post plating for mechanical strain.

The concept is that whisker growth rate is a function of stress resulting
from the exact manner of the coating growth. Plating electrochemistry which
imparts less stress is also known to be more stable in regard to whiskers.

Sorry, I don't remember the source of these coupons, but check Metal
Finishing magazine (they used to have a website).

Plating coupons which have right angle minimum radius bends in a dry
cabinet at 120-150 degrees C will accelerate the formation of whiskers
visible with 10X magnification into the range of a few days. They seem to
form first on the outer bend radii.


regards,




Jerry Cupples
Interphase Corporation
Dallas, TX USA
http://www.iphase.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2