Hi all,
What is the minimum vertical fill of solder for plated through holes ?
We have some problems to obtain the 75% requested by IPC-A-610 for a class 2
board.
In fact, the board has a thickness of 3,2 mm.
We use a no-clean flux and the wave is under nitrogen.
Is there any special criteria regarding to the thickness of the board ?
Has anyone succeeded in obtaining a correct solder filet for thick boards ?
Thanks,
Vincent Bada
Process Engineer
Alcatel Etca
Charleroi
Belgium
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|