There is Beta Backscatter, X-ray Fluorescence And Cross sectional
analysis using a high powered microscope with a reticle.We have both Beta
Backscatter and X-ray Fluporescence equipment from Veeco Instruments for
measuring plating thicknesses.
-----Original Message-----
From: Brian Gaynor [mailto:[log in to unmask]]
Sent: Tuesday, September 14, 1999 3:53 AM
To: [log in to unmask]
Subject: [TN] Measuring copper thickness @ incoming inspection
Hi,
What devices or techniques do you know of that can measure the thickness
of external & internal copper on a PWB from a PWB Manufacturer that does not
involve micro-section?
Best regards,
Brian Gaynor
Artesyn Technologies Europe.
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|