Jorge,
I have tried this technique before. It works fine till some paste
accumulates in the stencil apertures then I am back to square one. This also
would not help me much with glue applications.
Loan,
Turn fiducials into holes? As I recall Fuji GSP camera reads the
stencil from squeegee side. Right?
Trying this with MPM is same as teaching the pads and if you tape off
the holes from the bottom of stencil to avoid paste from getting into
everything it will create many other issues!
Ahne,
The engraving method sounds real good. I will definitely look into
it.
Thx everybody for your inputs. Ain't this grant. You "aks" a question and
here comes the wonderful answers purring down. And they say life is hard.
> -----Original Message-----
> From: Jorge Engenharia [SMTP:[log in to unmask]]
> Sent: Friday, September 24, 1999 8:54 AM
> To: [log in to unmask]
> Subject: Re: [TN] Fiducials
>
> Taheri;
>
> Some stencil printers ( MPM is one of then ) can use pad as fiducial,
> if
> your aplication is not critical ( no fine pitch devices ) you can use this
> option without any problem. I worked with pad as fiducial for years with
> no
> problem of misregistration, you have only to choose pads large enough to
> avoid solder acumulation in stencil aperture walls that can compromisse
> aligment.
>
> Thanx
> Jorge Dourado de Santana
> Maintenance / Process Engr
> Microtec - Brazil
>
>
>
> > -----Original Message-----
> > From: Tempea, Ioan [SMTP:[log in to unmask]]
> > Sent: 22 de Setembro de 1999 18:28
> > To: [log in to unmask]
> > Subject: Re: [TN] Fiducials
> >
> > Taheri,
> >
> > why don't you try to turn the fiducials into holes? Instead of cutting
> > half
> > of the thickness, have your stencil fab pierce the foil. And you don't
> > have
> > to fill.
> >
> > We are working like that for years on our Fuji GSP without the slightest
> > problem. This will also fix cleaning problems.
> >
> > Ioan
> >
> > > -----Original Message-----
> > > From: Taheri, Kamran [SMTP:[log in to unmask]]
> > > Sent: Wednesday, September 22, 1999 4:29 PM
> > > To: [log in to unmask]
> > > Subject: [TN] Fiducials
> > >
> > > Is there any other methods of putting fiducials on the stencil? Our
> > vender
> > > Laser cuts the fiducials half the thickness of the stencil then fills
> it
> > > with black adhesive. After a while the black adhesive starts to
> > > deteriorate
> > > and my phone rings of the hook. I usually get good results filling the
> > > fiducials on the thicker stencils with Loctite 410 black adhesive. But
> > not
> > > much luck when dealing with 5 or 6 mils thick stencils. Any comments
> > > appreciated.
> > >
> > > ##############################################################
> > > TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> > > ##############################################################
> > > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > > following text in
> > > the body:
> > > To subscribe: SUBSCRIBE TECHNET <your full name>
> > > To unsubscribe: SIGNOFF TECHNET
> > > ##############################################################
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > > additional
> > > information.
> > > If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask]
> > or
> > > 847-509-9700 ext.5365
> > > ##############################################################
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> > 847-509-9700 ext.5365
> > ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|