John,
The flux activity should conform to IPC J-STD 004, sect. 1.2 Table 1.
Your suppliers should list this on their Technical Data Sheets.
VBK
Vincent B. Kinol CQE
Applications Engineer
OMG Americas Microbond
[log in to unmask]
Phone 919-544-8090 x298
FAX 919-544-8090
-----Original Message-----
From: John Harris [SMTP:[log in to unmask]]
Sent: Wednesday, September 01, 1999 11:48 PM
To: [log in to unmask]
Subject: [TN] Flux activity
All,
Pardon my ignorance, but is there an industry standard for
specifying the "activity" of no-clean fluxes? I am looking for a way to
evaluate different fluxes that is more specific than simply their solids
content.
Any guidance would be greatly appreciated.
John Harris
Process Engineering
AEMS Pty Ltd
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|