Jason,
Are you speaking of surface or insertion mount solder joints? Are
you concerned about assembly issues (ie, will the joint fail during
wave solder), defect issues (will I create a void or a crack during
my process), or lifetime issues (what is the optimum size/shape for
long life?).
At CALCE we have a number of simulation tools that might be able to
help you with your query. Send me more information about what
inputs you have and what outputs you are interested in.
Regards,
Craig
> Is there anywhere I can obtain a model for predicting the life, strength, etc.
> of a solder joint? I would like to be able to input data one of two ways to
> determine what I can expect.
>
> 1. Can I input characteristics of the joint into some type of matrix i.e, hole
> size, plating thk, hole fill, fillet concavity, and get a life prediction model?
>
> 2. From FEM, obtain predicted overall stress and strain for the joint then
> extrapolate out into some life prediction model for reliability.
>
> My primary concern are joints on the bottomside of a PCB either from wave solder
> or the paste-in-hole process. I would appreciate direction or something
> another.
>
> Jason Smith
> Process Materials Engineer
> Lexmark Electronics
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
Dr. Craig Hillman
CALCE Electronic Products and Systems Consortium
University of Maryland
College Park, MD 20742
(301)-405-5316
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|