In a message dated 09/21/99 11:57:58, [log in to unmask] writes:
>Hi technetters
>Dos anybody knows where can I perform some thermal cycle test?
>Test conditions are 0-100 ºC and dewell time is 30 min.
>The maximum number of cycles will be around 1500.
>Any comment will be appreciated
>Alejandro Becerra
Hi Alejandro,
Any number of commercial test labs can perform this test; just look them up
in the IPC Membership Directory under Suppliers-Testing Services.
1500 maximum cycles indicates a rather benign application (according to
IPC-SM-785), so why bother testing. Analytical 'Design for Reliability'
procedures (IPC-D-279) assure reliability equally as well and are much
cheaper.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|