We changed to vacuum oven, because of too much built-in voids when conveyor soldered. That was large semiconductor chips for heatspreaders (the metal plating outgassed). X-ray showed significant improvement. To get max wetting, we also plasma clean heatspreaders before assembly starts. Guess you ask for semi chips also. Don't know what help this may give you...
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: JEFF PERKINS [mailto:[log in to unmask]]
Sent: den 17 september 1999 18:36
To: [log in to unmask]
Subject: [TN] Fluxless soldering (AuSn) with SMT reflow ovens
Is anyone doing fluxless soldering with AuSn eutectic preforms in SMT reflow ovens (inline conveyor, not batch)?
Any problem achieving temperature (eutectic point 280C)?
Any problems in Nitrogen environment?
How about preforms of other compositions?
Thanks,
Jeff Perkins
Epitaxx
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|