You are depleting the additive - try add about 10 to 15 % of additive
content and check.
Anil kher
----- Original Message -----
From: Francis Lai <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 16, 1999 11:05 AM
Subject: [TN] Dull finish around holes in Cu plating
> We are using pattern plating. After carbon treatment of our acid plating
> bath, we ran dummies for 2 hours then plate our panels. However the area
> around the holes showed dull and slightly rough finishes. The areas
> which have no holes showed shiny. We use the plating bar method. We
> etched the pattern and then use platting bar for connections. We ran two
> panels in a bath which was not carbon treated and they were fine. The
> PTH walls looked dull and slightly rough too. Can anyone help?
>
> My e-mail : [log in to unmask]
>
> Thanks!!!!!
>
> Francis
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|