I don't recommend filling with anything. Vias that small, and shallow, allow
solder paste deposition and solderability, minus some possible outgassing.
Besides, plating 1 mil minimum copper thickness almost makes them plate
closed.
Earl Moon
----- Original Message -----
From: edward Edward Szpruch <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 14, 1999 5:01 AM
Subject: [TN] BGA micro-blind vias
> Hi,
> What is the common practice concerning blind-microvias located on BGA
pads:
> a) open ? ( 2-3 mills diameter, 2 mills deep)
> b) filled with what ( fill materials,LPI solder mask)?
> c) filled with electroplated copper ?
> Pls advice
>
> Edward Szpruch
> Eltek , Manager of Process Engineering
> P.O.Box 159 ; 49101 Petah Tikva Israel
> Tel ++972 3 9395050 , Fax ++972 3 9309581
> e-mail [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|