If you're talking Alpha Level process (?):
1
good solderability (as HASL(even no cleans bite well) , planarity .
2
they don't hold as well in store as NiAu (say use within 6 months sealed)
3
very sensitive (more than osp!) on touch ; the finger acid breaks the seal
and than the silver tarnishes very fast.
4
doesn't like multipass (obviously) ; experiment prior to double side process
.
-----Original Message-----
From: Carl Ray [mailto:[log in to unmask]]
Sent: Saturday, 11 September 1999 21:41
To: [log in to unmask]
Subject: [TN] SMOBC Explain
Hey Guys,
Got a question. I have to start running some PCBs that have Organo-Metallic
Silver Immersion for plating. What are the pros and cons? Will I have to use
OA solder paste? Any information will be beneficial.
Carl Ray
Engineering Supervisor
256-494-3247 Direct line
256-492-8997 ext. 272
256-494-0625 Fax
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|