Cecilia,
From past experiences, I found that two of the major Si adhesive producers
both had "left over" monomers in theior adhesives, and gels, even when fully
cured, Unless the manufacturers make their product truely stochiometric, there
will be something free to float about in the product case. When I quizzed them
about this, and asked for weight loss data etc, they both promised the stuff,
and then went mysteriously quiet. I guess some of the more polymer oriented
folks on TN will be able to help more!!
Roger
Motorola AIEG
______________________________ Reply Separator _________________________________
Subject: [TN] Silicon and eletronic production
Author: "TechNet E-Mail Forum." <[log in to unmask]> at #email
Date: 10/09/99 10:47
Hello!
What is the stat of the art regarding silicon adhesives and any silicon products
in the electronics industry?
Our company has a strong restriction against any silicon. Has the adhesives etc
improved so that no monomers etc can evaporate?
Cecilia Alkhagen
******************************************
Ericsson Microwave Systems AB
Production Engineering Development
Bergfotsgatan 2
S-431 84 Mölndal
Telephone +46 31 747 0000
Direct +46 31 747 0288
Fax +46 31 747 2635
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|