Does anyone know what the minimum acceptable solder joint shear strengths
are for Sn63/Pb37 and In50/Pb50 ?
We are trying to optimize our soldering to gold interconnect process and
need some baseline/ industry standard numbers.
Thanks
Ron VandenDolder
Operations Manager
Millitech Corp
[log in to unmask]
##############################################################