Subject: | |
From: | |
Reply To: | |
Date: | Thu, 5 Aug 1999 18:07:45 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
My company tested diamond coated drill bits with Ted Gains at Pronto
Circuit Technologies. Megatool #68 bits were coated and the hits
increased from 5000 to 10,000. PCT does not have the time to do a
higher volume test and I am looking for other companies who would like
to test the diamond coated bits. I have many Megatool #68 coated bits
on hand that I will send for free. I can coat any manufactures bits.
If you have any questions or suggestions please email or contact me at
the number below.
Russell Epstein
President
Advanced Industrial Ceramics
12651 Briar Forest, Suite 151
Houston, Tx 77077
[log in to unmask]
Tel: 800-865-0532
Tel: 281-497-4788
Fax: 281-556-9244
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|