IPA (Isopropanol) will strip acrylic conformal coating without affecting
epoxy. If time is of the essence, stronger solvents may be added to the IPA
in small amounts to accelerate the process. This works only on true AR
coatings, which are lacquers (i.e., no cross-linking occurs in curing). The
AR\UR Hybrids are totally different animals.