I agree with Joe's suggestion of trying ACS. They're in Temecula. CA. They
make thin core processors and the noise they produce is lower than many
doing the same thing. Also, like Joe mentioned, many shops are still using
batch oxide processing lines and drying in a turbine dryer or an oven. Many
are moving on to new oxide alternative products or at least conveyorized
oxide lines. And there are several manufacturers of processing lines, most
of which I'm sure you're familiar with. All of them would most likely sell
stand-alone dryers.
Mark Mazzoli
Circuit Technologies
Atlanta, GA
770-458-1700
----- Original Message -----
From: Hinners Hans CIV WRALC/LYPME <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, August 17, 1999 11:44 AM
Subject: [TN] Any Recommendations on Board Dryers
> Hi All,
>
> I'm looking for recommendations on board dryers.
>
> We do thin inner layers and flex (a couple of mils) through pretty thick
> multilayered boards say ~150 mils.
>
> I'm very interested in quiet. The ones we have now can be heard from
> several hallways away and ear protection is required if you are in the
room.
>
> What do folks use to dry oxided panels?
>
> Hans
>
>
> Air Force Material Command - We keep them flying!
> ~~~~~~~~
> Hans M. Hinners WR-ALC/LYPME Bldg. 640
> Materials Engineer 380 Second Street,
> Suite 104
> Manufacturing Eng. Sec. Robins AFB GA 31098-1638
> 912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|