Title of Specification MIL-G-45204C is Gold Plating,
Electrodeposited this Specification has been cancelled.
Type II means 99.0 percent gold minimum
Grade C means Koop hardness 130-200, incl.
Class 00 means 0.00002 inch thick, minimum
The Specification is silent on amount of nickle underplate other
than saying it maybe used.
Date sent: Fri, 27 Aug 1999 10:50:01 -0700
Send reply to: "TechNet E-Mail Forum." <[log in to unmask]>,
TPE Engineering TechNet <[log in to unmask]>
From: TPE Engineering TechNet <[log in to unmask]>
Subject: [TN] Mil-G-45204
To: [log in to unmask]
> I have a drawing that requires keypads to be plated with
> gold. This drawing references MIL-G-45204, type 2, grade C
> class 00. What type of gold is this? Electrolytic, immersion
> or electroless. How much nickel is required to be plated
> under this gold? Any help I can get on this would be
> appreciated.
> Thanks,
> Ron Hayashi
> Toppan Electronics
> 1-858-695-2222, ext. 243
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ############################################################## To
> subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To
> unsubscribe: SIGNOFF TECHNET
> ############################################################## Please
> visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information. If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or 847-509-9700 ext.5365
> ##############################################################
Bob Haynes
Manager Of Design Engineering
General Atronics Corporation
1200 E Mermaid Lane
Wyndmoor PA 19038
Telephone 215-242-7273
FAX 215-233-9947
email [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|