Hi Eric - take a look at IPC specification ANSIJ-STD-002A for the
solderability and wetting information you are looking for!
Dave Hillman
Rockwell Collins
[log in to unmask]
Eric Lodangco <[log in to unmask]> on 08/13/99 04:42:42 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Eric Lodangco <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] Solder Dipping Process
Hello people;
We have a new process to be implemented on our 600 mil DIPs w/c is solder
dip them using 63/37 solder after component preparation (shear and splay).
Need to know more on standard or the criteria for:
1. Solderability
2. Wetting
3. De-wetting
4. Flux residue
5. STD plating thickness and composition
Thanks. Your valuable inputs are highly appreciated.
Eric
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################