Since there are "no dumb questions": I need to properly designate a
Cu-Mo-Cu material specification for a board that is 0.889 inch thick. This
would yield 35.56 increments of 0.025mm - for the IPC-CF-152/5 CICWxS
designation, should "x" be rounded to, say, 36 or left with the decimals ?
Thank you kindly.
##############################################################